Moisture uptake can affect flow and assay results. Record the bag materials, liner, closure, filling atmosphere and any damage on arrival. These observations complement a specification for the film itself.
A 25 kg shipment with a damaged liner
An outer 25 kg bag can look intact while its inner layer is punctured. Inspect seals and accessible liner surfaces at receiving. Record the temperature and relative humidity used for the film’s water-vapour transmission test. A film value will not reveal a faulty seam or closure.